Blow-out failure: failure is characterised from the lateral spalling of concrete inside the proximity on the anchor's head. This sort of failure occurs for anchors (prevalently Forged-in-spot) installed near the edge of the concrete ingredient.Sebaiknya terbuat dari besi beton ulir. Namun, jika hal tersebut tidak terlaksana oleh sesuatu hal. Solusi